Digital Library Publications
Predicted & Measured Glass Surface Temperatures In An Industrial, Regeneratively Gas-Fired Flat Glass Furnace
R R Hayes Et Al
Special Glass
Predicted And Measured Glass Surface Temperatures In An Industrial, Regeneratively Gas-Fired Flat Glass Furnace
R R Hayes Et Al
Special Glass
Validation Of An Improved Batch Model In A Coupled Combustion Space/Melt Tank/Batch Melting Glass Furnace Simulation
J Wang Et Al