Sensor Innovation For Burner Control In Glass Furnaces

In this article, the authors discuss the development and benefits of a non-invasive sensor that provides average, representative values for both the CO and O2 concentrations over the cross-section of flue gas channels.

Author
A J Faber & M Van Kersbergen
Origin
Celsian Glass & Solar, Netherlands
Journal Title
Glass Worldwide Nov-Dec 2016 110-113
Sector
General
Class
G 4531

Request article (free for British Glass members)