Role Of Atomistic Simulations In Understanding Fission Product Accommodation In Ceramic Nuclear Fuel

This article examines the design of longer lived nuclear fuel pellets, which requires accurate understanding of how microstructures accommodate fission products.

Author
S B Sinnott & B P Uberuaga
Origin
Cams & University Florida
Journal Title
Am Ceram Soc Bull 93 2 2014 28-32