Determination Of The Viscosity-Temperature Curve For Glasses Ont He Basis Of Fixed Viscosity Points Determined By Hot Stage Microscopy

This work establishes a method for obtaining the viscosity-temperature curve for glasses on the basis of the characteristic points obtained by hot stage microscopy and the comparison with the viscosity-temperature curves measured with a high temperature viscometer.

Author
M J Pascual Et Al
Origin
Csic, Spain
Journal Title
Phys Chem Glasses 42 1 2001 61-66
Sector
Special Glass
Class
S 2153

Request article (free for British Glass members)

Determination Of The Viscosity-Temperature Curve For Glasses Ont He Basis Of Fixed Viscosity Points Determined By Hot Stage Microscopy
Phys Chem Glasses 42 1 2001 61-66
S 2153