Chemical Treatment Of Glass Substrates

The effects of cleaning on the near-surface composition of Corning Code 1737 glass was studied. Cleaned glass substrates were found to develop a thin silica-rich surface layer approximately 6nm thick formed by chemical leaching. The presence of this layer was verified by X-ray photoelectron spectroscopy, scanning transmission electron microscopy and X-ray scattering. Atomic force microscopy measurements of the glass before and after cleaning showed no increase in the surface roughness.

Author
J G Couillard Et Al
Origin
Cornell University, Usa
Journal Title
Corning Research 1997 7-12
Sector
Special Glass
Class
S 1544

Request article (free for British Glass members)

Chemical Treatment Of Glass Substrates
Corning Research 1997 7-12
S 1544