Some of the man-made objects (beads, pieces of bangles/rings, and slag fragments) dating as far back as 700 B.C. and recovered in the Nevasa excavations have been analysed using an electron microprobe analyser.
Origin
Alfred University, Corning Glass Works, Deccan College
Journal Title
Trans Indian Ceram Soc 1988 47 5 149-155
Sector
Special Glass
Class
S 271