Digital Library Publications
British Glass has the UK’s only dedicated library on glass technology, from raw materials to end product. We collect and catalogue materials from sources including scientific journals, trade press, conference proceedings, standard setting bodies and more.
Each month our library and information service answers hundreds of enquiries from members – providing hand-picked information to help them meet their business needs. We particularly specialise in providing:
- worldwide legislation, regulations, standards and guidelines – such as heavy metals, decoration, food contact
- statistics – eg import/export data and recycling rates
- factory data – including types of glass manufactured, production capacities
- technical information on glass manufacture, material science, production techniques, compositions, decoration
- patents – including searches going back to the 19th century.
If there is something specific we can help with, email [email protected]
If you're not a member, we may still be able to help. Get in touch to find out more.
You can search our online database of articles, view abstracts, and order copies of articles using the search function below.
View our latest abstracts
Thermal Stability Of Lithium Metasilicate Produced Under High Pressure From Lithium Disilicate Glass
Dr S Buchner Et Al
Special Glass
The Structure Of Rhenium-Containing Sodium Alumino (Iron) Phosphate Glasses
S V Stefanovsky Et Al
Special Glass
The Glassy Area, Structure And Some Properties Of Glasses On The Zrf4 Basis
L Samek Et Al
Special Glass
Tb3+ As Probe Ion - Clustering And Phase Separation In Borate And Borosilicate Glasses
A Herrmann Et Al
Special Glass
Sulphur Solubility In Low Activity Waste Glass And Its Correlation To Melter Tolerance
C H Skidmore Et Al
Special Glass
Structure, Properties, And Fabrication Of Calcium Aluminate-Based Glasses
Y Lin Et Al
Special Glass