Digital Library Publications
British Glass has the UK’s only dedicated library on glass technology, from raw materials to end product. We collect and catalogue materials from sources including scientific journals, trade press, conference proceedings, standard setting bodies and more.
Each month our library and information service answers hundreds of enquiries from members – providing hand-picked information to help them meet their business needs. We particularly specialise in providing:
- worldwide legislation, regulations, standards and guidelines – such as heavy metals, decoration, food contact
- statistics – eg import/export data and recycling rates
- factory data – including types of glass manufactured, production capacities
- technical information on glass manufacture, material science, production techniques, compositions, decoration
- patents – including searches going back to the 19th century.
If there is something specific we can help with, email [email protected]
If you're not a member, we may still be able to help. Get in touch to find out more.
You can search our online database of articles, view abstracts, and order copies of articles using the search function below.
View our latest abstracts
Helium Permeation, Diffusion And Solubility In Sodium Galliosilicate Glasses
J C Lapp & J E Shelby
Special Glass
Formation And Properties Of Sodium Scandium Silicate Glasses
J E Shelby & J J Noonan
Special Glass
Structure And Nonlinear Optical Properties Of Lanthanide Borate Glasses
K Terashima Et Al
Special Glass
Effect Of Refining Agents On Reboil Caused By Stirring Glass Melts (In Japanese)
H Kushitani Et Al
Special Glass