Digital Library Publications
British Glass has the UK’s only dedicated library on glass technology, from raw materials to end product. We collect and catalogue materials from sources including scientific journals, trade press, conference proceedings, standard setting bodies and more.
Each month our library and information service answers hundreds of enquiries from members – providing hand-picked information to help them meet their business needs. We particularly specialise in providing:
- worldwide legislation, regulations, standards and guidelines – such as heavy metals, decoration, food contact
- statistics – eg import/export data and recycling rates
- factory data – including types of glass manufactured, production capacities
- technical information on glass manufacture, material science, production techniques, compositions, decoration
- patents – including searches going back to the 19th century.
If there is something specific we can help with, email information@britglass.co.uk
If you're not a member, we may still be able to help. Get in touch to find out more.
You can search our online database of articles, view abstracts, and order copies of articles using the search function below.
View our latest abstracts
Addition Of Fluorospar As A Means Of Increasing The Output Of Mechnised Plants For Sheet Glass.
D.L. Gik.
Primary Papers
Vitrification And Properties Of Glasses On Fluorophosphate Systems Containing 3 D-Elements (Russian)
T.M. Rozanov And V.D. Khalilev
Primary Papers
Efect Of Flourine And Phosphorous Pentoxide On Properties Of Soda-Dolomite Lime-Silica Glass.
Owens-Illinois Glass Company General Research Lab
Primary Papers
Relative Speed Of Melting Of The Glass Blends With Boric Acid And Borax.
F.H Zschacke And J. Vertanian
Primary Papers
Application Of Ion Exchangers In Analytical Chemisty Of Silicates. The Determination Of Fluorine In Fluorine-Glasses.
M. Palecek
Primary Papers
Effect Fo Fluorine Associated With Other Minor Batch Constituents On Some Properties Of Commercial Glasses.
Stephane De Lajarte
Primary Papers
Spectrophotometric Method Of Determining Fluorine In Glasses After Seperation By Pyrohydrolosis
P. Mayaux And R. Renson-Salme
Primary Papers