X-Ray Photoelectron Spectroscopy Of (100-X)(0.6Li2S.0.4Sis2).Xli4Si04 Oxysulphide Glasses

S2p and 01s photoelectron spectra were mesured for the (100-x)(0.6Li2S.0.4SiS2).xLi4Si04(x=0.5,10,15,20) oxysulphide glasses. In the 95(0.6Li2S.04SiS2).5Li4Si04 glass, 92% of sulphur atoms were present as nonbridging ones and 85% of oxygen atoms were present as bridging ones.

Author
A Hayashi Et Al
Origin
Osaka Prefecture University, Sakai, Japan
Journal Title
Phys Chem Glasses 39 3 1998 145-150