The X Ray Fluorescence Analysis Of Glass And Glass Batches. The Effects Of The Volatile Constituents And The Effects Of The Adjacent Spectral Lines.(In Polish)

XRF analysis of sheet glass is discussed with particular reference to the absorption effects of Al, the interdependence of K and Ca and the effect of Si in the determination of Al using a lithium borate fusion technique for bead preparation.