Worlds Largest Safety Glass Plant

Klopper Maschinentechnik has delivered what it believes to currently be the world's largest laminated safety glass plant to a Japanese glass manufacturer who wants to use the plant for triple combines, with an individual plate thickness of 25mm and in a 3.21 x 12.0m format. (whole item)