Worlds Largest Float Plant

The PPG float glass plant at Carlisle Pa. which has three hundred million square feet of glass per year is described briefly.

Author
Anon
Origin
Unknown
Journal Title
Glass 1972 52 (5) 8-10
Sector
Primary Papers
Class
PP 456

Request article (free for British Glass members)

Worlds Largest Float Plant
Glass 1972 52 (5) 8-10
PP 456