Why Do We Make Glass So Weak? A Review Of Research On Damage Mechanisms

The state of knowledge of damage mechanisms is reviewed and information obtained in laboratory studies is related to that obtained from studies of the strength of glassware. The significance of the data for glass manufacturing processes is also discussed.