The Waste Swap: One Way To Minimize

For any manufacturer, there are basically four opportunities to minimize waste going to landfill or incinerator. First, don't create it! Second, recycle waste within your own factory or industry sector. Third, import waste from another industry. Fourth, export waste to another industry. This article focuses on a research and development project aimed at showing that waste bottle glass can be used as a flux in brick bodies.

Author
Un-named
Origin
Unknown
Journal Title
Int Ceramics 1/2003 16-17, 19
Sector
General
Class
G 2638

Request article (free for British Glass members)

The Waste Swap: One Way To Minimize
Int Ceramics 1/2003 16-17, 19
G 2638