[Ware Handling] Customised Stacker Bar Benefits

Stacker bars warping as a result of prolonged exposure to heat can leave rows of glass containers curved and lead to uneven spray-on coatings. Such failures can result in thousands of dollars in losses, especially if a plant has to dump a lehr full of glass because of surface defects.