Visionary Inspection

The increased demand for high quality glass tubes for pharmaceutical glass or solar heaters has led to higher inspection requirements. The tube ends in particular, where the tubes have been cut, formed and fused with a heat treatment, require high quality levels. This article outlines a tube end inspection system able to process 18,000 tubes an hour.