Uvekol - The Cure For The Common Glass

For fabricators working with laminated glass, there are many areas where improvements in efficiency and consistency could be made.

Author
E Jenkins
Origin
Ucb Chemicals Corp
Journal Title
Glass Industry Development Int 2001 103