Using Glass Cullet In Electrical Ceramics

The use of TV glass cullet in the manufacture of low-voltage porcelain insulators is described.

Author
L P Gabrikova Et Al
Origin
All Union Scientific-Research Inst Of Electrical Ceramics
Journal Title
Glass And Ceramics 1987 44 7-8 278-282