Use Of Robotics In Crystal Ware Decoration

Aspects of training and using robots in cutting diamond facets on crystal ware and automated correction of the program related to deviations in product dimensions are studied. Technical and economic parameters of the process are given.

Author
N F Gerasimovich
Origin
Neman Glass Factory, Belarus
Journal Title
Glass And Ceramics 57 1-2 2000 69 - 72
Sector
Domestic glass
Class
D 982