Usage Of Cold Bent Glass Panes As An Approximation For Double-Curved Surfaces

After describing the growing usage of cold bent tempered architectural glass in the Netherlands, the author elaborates on material behaviour and geometrical characteristics of cold bending, which is illustrated with details, prototypes and realised applications.