Ultrasonic Spray Protection Of Float Glass

This article discusses the role of ultrasonic spray technology in the anti-strain protection of primary and coated float glass materials during transportation and storage.

Author
C Reifenberger
Origin
Sono-Tek, Usa
Journal Title
Glass Worldwide May-June 2013 88-89
Sector
Flat glass
Class
F 3396

Request article (free for British Glass members)

Ultrasonic Spray Protection Of Float Glass
Glass Worldwide May-June 2013 88-89
F 3396