The Trouble With Bent Glass

The use of large, bent glass by architects has not shown the same level of growth as that seen in the automotive glass and appliance sectors. This has been partly because of the product itself and partly because of the customers' perceptions of it. Here the author outlines the most persistent problems and the technical solutions available.