Triple Glazing: A Hot Debate

A number of recent articles and debate around triple glazing have highlighted the need for simple comparisons between the alternative glazing products and configurations possible for a site or location. In this article, the author, Garry Smith from Glass Technology Services discusses effective U values.

Author
G Smith
Origin
Glass Technology Services
Journal Title
Glass International May 2014 42
Sector
Flat glass
Class
F 3580