Transfers Keep Moving On The Right Line

Recently, both Emhart and Rockware are understood to have questioned the ability to operate the Sheppee transfer system and Emhart EFRA Flexline drive system on the same glass container production line. This article explains how the company has resolved this doubt and successfully integrated its transfer with the EFRA system.