Toughening And Tempering Lines

Increasing demand for higher quality in tableware and industrial products like isolators and vehicle headlights has driven producers to develop tempering lines for glass treatment, replacing annealing lehrs. In keeping with this industry trend CMT of France has developed technology that effect high-quality glass tempering.