Tinted Glazes Containing Float Waste

An opacified tinted glaze for facing tiles has been obtained on the basis of float-waste from a copper-concentrating factory. The optimum glaze compositions with good physico-chemical properties are identified.

Author
M T Mukhamedzhanova & A Irkakhodzhaeva
Origin
Academy Sciences, Uzbekistan
Journal Title
Glass & Ceramics 61 1-2 2004 30-31