Thermally Induced Fast Fracture In A Glass Double-Cantilever-Beam Specimen

Rapid crack propagation and arrest in a soda-lime glass double-cantilever-beam specimen subjected to a thermal shock loading are investigated. The crack growth-time history is measured and compared with that predicted by a one-dimensional dynamic fracture model.