Thermal Conductivity Of Some Titania And Lithia Glasses

Thermal conductivity of eleven glasses of compositions SiO2 75 to 82.4 TiO2 to 8.1 and Li2O 16.17 to 17.6 wt% was measured. Factors for the specific contribution of SiO2, TiO2 and LiO2 to the thermal conductivity were calculated. The factors were f SiO2 3.2 f TiO2 -7.5 and f Li2O -2.22 cal cm-1 sec-1 deg-1 c.

Author
M.M. Ammar Et Al
Origin
Unknown
Journal Title
Central Glass And Ceramic Research Institute Bulletin 1975 22 (1) 10-13