Theoretical Estimation Of The Possibility Of Glass Formation In The Sulfate, Phosphate, And Sulfate-Phosphate Systems

The possibility of preparing glasses in sulfate, phosphate, and sulfate-phosphate systems is estimated from nine criteria of glass formation. It is shown that if these criteria concern only the first coordination sphere (i.e. the formation of P04 and S04 groups), glass formation in the systems should be considered possible. The majority of the criteria of glass formation have a defect consisting of the fact that their use is necessary but not sufficient for predicting the possibility of preparing glasses in a wide class of systems.

Author
V L Mamoshin
Origin
Unknown
Journal Title
Glass & Ceramics 53 3-4 1996 104-106
Sector
Special Glass
Class
S 1524

Request article (free for British Glass members)

Theoretical Estimation Of The Possibility Of Glass Formation In The Sulfate, Phosphate, And Sulfate-Phosphate Systems
Glass & Ceramics 53 3-4 1996 104-106
S 1524
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.