Temperature Measurement In The Glass Industry Using Radiation Thermometers

A review of infrared thermometers and their application, installation and maintenance for measuring the temperature of regenerator packings, crown, bridgewalls, port arches, tank roof and forehearths.

Author
D Dixon
Origin
Land Infrared, Uk
Journal Title
Fundamentals Of The Glass Manufacturing Process 1991. Esg Conf. 163-165
Sector
Container glass
Class
C 613