Tasks, Problems And Scientific Results Of Absorption Of Waste Gases Containing Fluoride In The Glass Industry. (In German).

Fluoride emissions in the glass industry are discussed with particular reference to methods of analysis and possibilities of pollution reduction.

Author
J. Lange.
Origin
Unknown
Journal Title
Silikattechnik 1977 28 (6) 184-186