Tableware Decoration Product Development

The ability of colour manufacturers and decorators to respond to the ever-changing demands of the marketplace and their customers was discussed at the 1991 SGCD Annual Conference in Orlando, USA. This paper reviews a few specific aspects and how conformity to these requirements through new product developments can be continued.

Author
S Bennett
Origin
Johnson Matthey
Journal Title
Glass Machinery Plants & Accessories 6 3 1993 80-83