System Integration Solutions For The Glass Industry Featuring The Inex Information Interface System

In this article Inex Vision Systems will provide a presentation on one of their products namely, Inex Information Interface System. This is a computer-based network system that connects a variety of cold end inspection equipment. It provides sampling control, data acquisition and information displays to manufacturing personnel.