Swedish Closure

Swedish glass maker Orrefors have failed to find a new owner, sealing the company's plans to move production away from the country's Crystal Kingdom. It has been reported that all production will now end at the glassworks in Southwestern Sweden. Workers who have remained at the factory since owners New Wave Group announced its closure in October 2012 will get paid for their last week.