Swabbing Robot Success

In 2005, French company Novaxion created the fist swabbing robot in partnership with a global glass packaging manufacturer. Today, with 37 units already operating in glass plants throughout the world, the SR200 swabbing robot has proved to be a reliable and efficient swabbing solution for IS machines.