Surface Treatment - Diamondguard Scratch And Abrasion Resistant Glass

Guardian has developed the materials, processes and deposition equipment to deposit DLC films on large area glass substrates. DiamondGuard optical thin films demonstrate high scratch and abrasion resistance, optical transparency, low coefficient of friction, and high degrees of hardness. There are numerous applications for the DiamondGuard thin film technology. In addition to producing scratch and abrasion resistant glass, the DLC can be combined with other PVD techniques to product low maintenance or easy clean glass products with superior hardness and scratch resistance while exhibiting super-hydrophilic properties.

Author
Un-named
Origin
Unknown
Journal Title
Int Glass Review 1/2002 59-61
Sector
Flat glass
Class
F 1330

Request article (free for British Glass members)

Surface Treatment - Diamondguard Scratch And Abrasion Resistant Glass
Int Glass Review 1/2002 59-61
F 1330
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.