Surface Coatings - Sputter Targets For Large Area Coating

Planar versus rotatable technology - Marcus Wendel of Heraeus GmbH takes a materials point of view.

Author
M Wendel
Origin
Heraeus Gmbh, Germany
Journal Title
Glass Int 5 Sept-Oct/03 48-49
Sector
Flat glass
Class
F 1472