Suppliers Recommend Limiting Use Of Tempered Glass In Buildings

The advantages of heat-strengthened glass relative to toughened glass in glazing above ground level are discussed with particular reference to the possibility of "spontaneous" fracture due to nickel sulphide stones in toughened glass.