Supplier Installs Float Glass Line For Russian Manufacturer

Horn Glass Industries AG received an order for the complete execution of a new float glass line with a capacity of 600/tpd in 2004 for Salavatsteklo AG, one of the leading Russian manufacturers of float and container glass, tempered glass, safety glass, sodium water glass and other goods. The glass maker, which employs around 2500 people, is located in the foothills of the Ural mountains in the city of Salavat. Its products are successfully sold in Russia, as well as abroad. This article takes a look at the project.

Author
Un-named
Origin
Unknown
Journal Title
Glass May 2006 18
Sector
Flat glass
Class
F 2060

Request article (free for British Glass members)

Supplier Installs Float Glass Line For Russian Manufacturer
Glass May 2006 18
F 2060
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.