Optical flawlessness requires flat glass manufacturers to secure 100% defect-free products. The early detection of defects avoids costs through coating or tempering of plates, which are ultimately rejected. This article describes an optical inspection solution that allows for comprehensive quality surveillance and supplies the key to the best yield and competitively viable production.