Sunnier Outlook For Powerful Windows

According to this article, "Windows could soon be providing us with power, as well as letting in light." A team of chemists led by Michael Gratzel at the Swiss Federal Institute of Technology in Lausanne, have made a breakthrough in their pioneering design of a transparent solar cell so that it now converts 10% of the energy in sunlight into electricity.