Sunglasses, Pupil Dilation, And Solar Ultraviolet Irradiation Of The Human Lens And Retina

A survey of over 400 retail sunglass lenses of all types showed that all would reduce UV radiation densities in all parts of the crystalline lens and on the retina.

Author
H L Hoover
Origin
Corning Glass Works
Journal Title
Applied Optics 1987 26 689-695