Sulfur Chemistry In A Borosilicate Melt. Part 3. Iron-Sulphur Interactions And The Chromophore

The interactions of iron and sulphur in a borosilicate melt have been defined as a function of iron content, sulphur concentration, melt temperature and oxygen fugacity.