Subcritical Growth Of Indentation Median Cracks In Soda-Lime-Silica Glass

The invluence of load and dwell time on the subcritical growth of indentation cracks was investigated.

Author
V M Sglavo & D J Green
Origin
Pennsylvania State University, Usa
Journal Title
J Am Ceram Soc 78 3 1995 650-656
Sector
General
Class
G 1232