The Study On The Inclusion Of Se In The Bubbles In Glass Using Laser-Raman Spectral Analyser

The bubbles in glass which included the incusion of Se were observed under an optical microscope in order to determine the analytical microzone. Then, using laser Raman probe microzone analyser, the Raman spectrums of the standard Se crystal and industrial Se power were determined. Finally, the inclusions in the bubbles were analysed.