Study Of The Factors Responsible For Exudation Of The Glassy Phase In Azs Refractories

The influence of cyclical compared with sustained heating as a function of micropore formation is discussed. It is suggested that the dissolution of gases in AZS refractories is a major motive force for run-out of glassy phase.