Studies On The Flow Of Molten Glass In A Glass Tank By Model Technniques.

A model of a bridge-wall tank was made of plastics to the scale of 1/50, and molten glass was replaced by 82% glycerin. Grains of plastics covered with Al powder were used for observation of the velocity distribution in the flowing glycerin. The effects of heat input from the top surface and of the arrangement of heaters on the flow patterns and the temperature distribution were studied.