Structure Formation Of Cellular Heat-Insulation Material From Cold-Solidifying Liquid-Glass Composition

The possibility of obtaining foamed heat-insulation material at room temperature on the basis of liquid glass with calcium-containing additives is examined. A method of controlling gas generation and solidification of a liquid-glass composition by changing the silicate modulus of liquid glass is shown.

Author
V V Samoilenko & V V Firsov
Origin
Siberian Branch Russian Acad Sci
Journal Title
Glass & Ceramics 68 7-8 Nov/2011 250-252
Sector
Flat glass
Class
F 3201

Request article (free for British Glass members)

Structure Formation Of Cellular Heat-Insulation Material From Cold-Solidifying Liquid-Glass Composition
Glass & Ceramics 68 7-8 Nov/2011 250-252
F 3201