Structural Rearrangements In Silcate Glasses During Annealing

The equilibrium temperature coefficients of refractivity or optical sensitivity to prolonged annealing for 23 silicate glasses were plotted as functions of chemical compositions expressed as fractions of on silica on a basis varying from completely ionic fo lowest silica.